MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX918A Polyphenylene Ether + PA (PPE+Nylon)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 918A resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, excellent chemical resistance, high melt flow, and added mold release. NORYL GTX918A resin may be an excellent candidate for automotive under-the-hood and electrical applications requiring the retention of properties while under thermal load.

Features: Hydrolytic Stability,Chemical Resistance,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Flow,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/ccASTM D792
Moisture Absorption 0.0700 %Injection Molding
Water Absorption at Saturation 4.2 %ASTM D570
Viscosity 5.0 cP
@Load 1.20 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.013 - 0.016 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.010 - 0.013 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 45 g/10 min
@Load 5.00 kg,
Temperature 280 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
 57.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
 62.0 MPa50 mm/min; ASTM D638
Elongation at Break 30 %50 mm/min; ISO 527
 53 %50 mm/min; ASTM D638
Elongation at Yield 4.5 %50 mm/min; ISO 527
 11.4 %50 mm/min; ASTM D638
Flexural Strength 85.0 MPayield, 2 mm/min; ISO 178
 98.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2200 MPa2 mm/min; ISO 178
 2360 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 202 JASTM D256
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 20.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
Dart Drop, Total Energy 40.0 Jpeak; ASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 64.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 68.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.250 W/m-KASTM C177
Deflection Temperature at 0.46 MPa (66 psi) 185 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 188 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 148 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 190 °CRate B/50; ISO 306
 195 °CRate B/120; ISO 306
 242 °CRate B/50; ASTM D1525
 245 °CRate A/50; ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 295 °C
Zone 2 260 - 295 °C
Zone 3 265 - 295 °C
Melt Temperature 270 - 295 °CInjection Molding
Mold Temperature 65.0 - 95.0 °C
Drying Temperature 95.0 - 105 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Moisture Content 0.020 %minimum
Back Pressure 0.300 - 1.40 MPa
Shot Size 30 - 50 %
Vent Depth 0.00130 - 0.00380 cm
Screw Speed 20 - 100 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82165 / 290112

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.