MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Pressure Seal 20662 Fluorinated Silicone
Categories: Polymer; Thermoset; Silicone

Material Notes: Compound 20662 is a 60 durometer blue colored Fluorosilicone elastomer. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 609 A19 EO36 F19
MIL-R-25988 Class1, Grade 60, Type 1 & 11
AMS 3325

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.48 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 60
 48
@Temperature 23.0 °C,
Time 79200 sec
ASTM Reference Fuel B
 53
@Temperature 150 °C,
Time 252000 sec
Stauffer Blend 7700
 66
@Temperature 200 °C,
Time 252000 sec
Heat Aged
Tensile Strength 1146 psi
 875.5 psi
@Temperature 23.0 °C,
Time 79200 sec
ASTM Reference Fuel B
 928.3 psi
@Temperature 150 °C,
Time 252000 sec
Stauffer Blend 7700
 1135.7 psi
@Temperature 200 °C,
Time 252000 sec
Heat Aged
Elongation, Ultimate 330 %
 264 %
@Temperature 23.0 °C,
Time 79200 sec
ASTM Reference Fuel B
 269.9 %
@Temperature 200 °C,
Time 252000 sec
Heat Aged
 269.9 %
@Temperature 150 °C,
Time 252000 sec
Stauffer Blend 7700
Tear Strength 155 pliDie B
Compression Set 8.7 %
@Temperature 175 °C,
Time 79200 sec
Plied
 9.5 %
@Temperature 23.0 °C,
Time 252000 sec
Plied
 13.8 %
@Time 252000 sec
Stauffer Blend, plied
 
Thermal PropertiesOriginal ValueComments
Brittleness Temperature <= -80.0 °F
Shrinkage -1.00 %
@Temperature 200 °C,
Time 252000 sec
Weight, Heat Aged
 7.4 %
@Temperature 150 °C,
Time 252000 sec
Volume, Stauffer Blend 7700
 20.1 %
@Temperature 23.0 °C,
Time 79200 sec
Volume, ASTM Reference Fuel B
 
Descriptive Properties
ColorBlue

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPRESL214 / 318424

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.