Applications: Television shell, sound shell, shell of electronic injection molding products Modified Features: Flame retardant Product Features: Apply to gas assisted injection molding , comply with ROHS, good comprehensive performance, good heat stability and electrical property, and flame retardant grade is UL-94 V0 Information provided by Wuxi Kangxi Plastics Technology Co., Ltd. |