Polypropylene copolymer 15% glass fibers reinforced, chemically coupled, very good impact strength also at medium-low temperatures. Available: all colors, UV stabilized (L), heat stabilized (H), laser printable (LP), detergent stabilized (D).Information provided by Taro Plast S.p.a. |