MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Formosa Plastics Formolene® E922 Film HDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); High Density (HDPE); High Density Polyethylene (HDPE), Film Grade

Material Notes: High Density Polyethylene Medium Molecular Weight Bi-Modal Resin Designed for Film Applications

Formolene® E922 is a medium molecular weight grade of HDPE designed for good processing characteristics and good film stiffness for thin gauge film applications.

Formolene® E922 meets all requirements of the U.S. Food and Drug Administration as specified in 21 CFR 177.1520, covering safe use of polyolefin articles intended for direct food contact.

Applications: Shopping Bags, Trash Can Liners and Thin Film for Laminate Applications

Information provided by Formosa Plastics Corporation, USA

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.953 g/ccASTM D1505
Thickness 0.750 mil
Melt Flow 0.15 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 390 %ASTM D882
Film Elongation at Break, TD 640 %ASTM D882
Elmendorf Tear Strength MD 13 gASTM D1922
Elmendorf Tear Strength TD 220 gASTM D1922
Dart Drop Test 240 gASTM D1709
Film Tensile Strength at Break, MD 7500 psiASTM D882
Film Tensile Strength at Break, TD 7600 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Melting Point 132 °CDSC
 
Processing PropertiesOriginal ValueComments
Blow-up Ratio (BUR) 4.0
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for High Density Polyethylene (HDPE), Film Grade
Unipetrol PE HD LITEN® FB 85 HDPE
Chevron Phillips HiD® 9662 HDPE Blown Film Resin
Total Finathene® 53140 HDPE, blow molding, sheet
Petromont 1201 High Density Polyethylene Resin

PFPCPQ045 / 150277

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.