SD1100P powder is a high purity 4,4’-BPADA powder. When used in polyimide applications, SD1100P powder may offer performance improvements such as solubility of polyimides in organic solvents, lower water absorption, lower dielectric constant and lower dissipation factor. Information provided by SABIC |