MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger SPI

Ensinger TECAMID 6 FRT black Nylon 6, Flame Retardant
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced, Flame Retardant

Material Notes:
  • tested according to EN 45545
  • resistant to many oils, greases and fuels
  • good slide and wear properties
  • high strength
  • good machinability
Target Industries:
  • aircraft and aerospace technology
  • transportation
  • electronics
  • mechanical engineering
  • automotive industry

Information provided by Ensinger Inc.

Vendors: Ensinger High Performance Plastics withstand severe environments, resist harsh chemicals, and perform well in extreme temperatures. They offer weight savings that have potential to drive lower cost systems.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Ball Indentation Hardness 182 MPa26400 psiISO 2039-1
Tensile Strength 78.0 MPa11300 psi50mm/min; DIN EN ISO 527-2
Elongation at Break 4.0 %4.0 %50mm/min; DIN EN ISO 527-2
Elongation at Yield 4.0 %4.0 %50mm/min; DIN EN ISO 527-2
Modulus of Elasticity 4.20 GPa609 ksi1mm/min; DIN EN ISO 527-2
Flexural Strength 124 MPa
@Load 1.02 kg
18000 psi
@Load 2.25 lb
2mm/min; DIN EN ISO 178
Flexural Modulus 3.80 GPa
@Load 1.02 kg
551 ksi
@Load 2.25 lb
2mm/min; DIN EN ISO 178
Compressive Yield Strength  54.0 MPa
@Strain 2 %,
Load 1.02 kg
7830 psi
@Strain 2 %,
Load 2.25 lb
5mm/min; EN ISO 604
 95.0 MPa
@Strain 5.0 %,
Load 1.02 kg
13800 psi
@Strain 5.0 %,
Load 2.25 lb
5mm/min; EN ISO 604
Compressive Strength 27.0 MPa
@Strain 1 %,
Load 1.02 kg
3920 psi
@Strain 1 %,
Load 2.25 lb
5mm/min; EN ISO 604
Compressive Modulus 3.00 GPa
@Load 1.02 kg
435 ksi
@Load 2.25 lb
5mm/min; EN ISO 604
Charpy Impact Unnotched 6.20 J/cm²29.5 ft-lb/in²max. 7,5J; DIN EN ISO 179-1eU
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 70.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
38.9 µin/in-°F
@Temperature 73.4 - 140 °F
DIN EN ISO 11359-1;2
Melting Point 221 °C430 °FDIN EN ISO 11357
Maximum Service Temperature, Air 100 °C212 °Flong term
 160 °C320 °Fshort term
Glass Transition Temp, Tg 45.0 °C113 °FDIN EN ISO 11357
Flammability, UL94 V-0
@Thickness 1.50 mm
V-0
@Thickness 0.0591 in
DIN IEC 60695-11-10
 
Descriptive Properties
Colorblack opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PENSIN8163 / 319091

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.