MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Cotronics Duralco™ 132 500°F (260°C) Aluminum Filled Epoxy
Categories: Polymer; Thermoset; Epoxy; Epoxy, Thermally Conductive

Material Notes: Aluminum filled epoxy that cures at room temperature to form machinable, thermally conductive bond lines. High heat transfer. Can be supplied as a “non-sag” putty.

Applications: heat tacking, heat transfer, and heat sink applications, i.e. bonding copper coils to vessels to provide for rapid heating and cooling for critical chemical processes.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity 22000 cP
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+6 ohm-cm
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 40.0 BTU-in/hr-ft²-°F
Maximum Service Temperature, Air 500 °F
 
Processing PropertiesOriginal ValueComments
Cure Time 960 - 1440 min
@Temperature 93.3 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Cotronics Duralco™ 133 500°F (260°C) Aluminum Filled Epoxy
Cotronics Duralco™ 135 500°F (260°C) Aluminum Filled Epoxy
Dow SE 4450 THERMALLY CONDUCTIVE ADHESIVE
Cotronics Duralco™ 134 500°F (260°C) Aluminum Filled Epoxy
Cookson Group Plaskon® ALP-2 (188.pcs03) Thin Package Encapsulant

PCOTR0360 / 29058

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.