MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LEXAN™ Copolymer FST9405 PC (Asia)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: Lexan* FST9405 resin is a high flow PC Copolymer Resin, suitable for injection molding. This halogen-free flame retardant resin is OSU55/55 and FAR25.583 compliant and an ideal candidate foraircraft interior applications. Available in opaque colors.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.33 g/ccASTM D792
Density 1.33 g/ccISO 1183
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cmSABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cmSABIC method
Melt Flow 9.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D1238
 10 g/10 min
@Load 1.20 kg,
Temperature 300 °C
MVR [cc/10 min]; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPa50 mm/min; ISO 527
 70.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 77.0 MPa50 mm/min; ISO 527
 77.0 MPa50 mm/min; ASTM D638
Elongation at Break 75 %50 mm/min; ASTM D638
 95 %50 mm/min; ISO 527
Elongation at Yield 6.0 %50 mm/min; ASTM D638
 6.0 %50 mm/min; ISO 527
Tensile Modulus 2600 MPa5 mm/min; ASTM D638
 2600 MPa1 mm/min; ISO 527
Flexural Yield Strength 105 MPa2 mm/min; ISO 178
 115 MPa1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2500 MPa2 mm/min; ISO 178
 2700 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact, Notched 130 J/mASTM D256
 85.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
 12.0 kJ/m²80*10*3; ISO 180/1A
 9.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*3; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*3 sp=62mm; ISO 179/1eU
 NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched NBEdgew 80*10*4 sp=62mm; ISO 179/1eA
 NBEdgew 80*10*3 sp=62mm; ISO 179/1eA
 NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eA
Impact Test 130 JMultiaxial Impact; ISO 6603
Instrumented Impact Total Energy 60.0 JASTM D3763
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 60.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 104 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 105 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 94.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 95.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 113 °CRate B/120; ISO 306
 114 °CRate B/50; ASTM D1525
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 245 - 275 °CInjection Molding
Zone 1 230 - 250 °C
Zone 2 240 - 270 °CInjection Molding
Zone 3 250 - 280 °C
Melt Temperature 250 - 280 °CInjection Molding
Mold Temperature 50.0 - 80.0 °C
Drying Temperature 95.0 - 100 °CInjection Molding
Dry Time 6.00 - 8.00 hourInjection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 40 - 60 %
Vent Depth 0.00250 - 0.00760 cm
Screw Speed 40 - 70 rpm
 
Descriptive Properties
NBS Smoke Density, Flaming, Dmax<75ASTM E662
OSU total heat release (2 minute test)<55 kW-min/m²FAR 25.853
OSU peak heat release rate (5 minute test)<55 kW/m²FAR 25.853
Vertical Burn a (60s) passes at1 secFAR 25.853

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH91450 / 252574

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.