Temper: Nominal Grain Size 0.015 mm Fabrication Properties: Excellent Suitability – Soldering, Brazing, Spot Weld, Seam Weld, Butt Weld, Capacity for Being Cold Worked; Good Suitability – Oxyacetylene Welding; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed Common Fabrication Processes: Bending; Blanking; Forming; Resistance Welding; Seam and Butt Welding; Spot Welded Components; Stamping Typical uses: Resistance Weldable Brass Products |