MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Chemical Cilbond® 33A/33B Bonding Agent
Categories: Other Engineering Material

Material Notes: Cilbond 33A/33B is a two component adhesive system, which is mixed to produce a once-coat system. Cilbond 33A/33B is suitable for bonding fluoroelastomer compounds of all hardnesses to a variety of substrates including metals (either chemically treated or mechanically abraded) and thermoplastics, thermosets and fabrics. The Cilbond 33A/33B system will bond all the major grades of fluoroelastomers available including Viton®, Daiel®, Aflas® Technoflon® and Fluorel®, which are bisphenol or amine cured and may also bond some peroxide cured fluoroelastomers and even some fluorosilicones, especially if post cured.

Information provided by HB Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/cc33B
 0.970 g/cc33A
Solids Content 19.1 %33B
 32 %Combined
 38.4 %33A
Volatiles 57 %33A
 78 %33B
Viscosity Measurement 16[sec], No 2 Zahn Cup, Combined
 15
@Temperature 25.6 °C
[sec], No 2 Zahn Cup, 33B
 16
@Temperature 25.6 °C
[sec], No 2 Zahn Cup, 33A
 
Thermal PropertiesOriginal ValueComments
Flash Point 17.6 °FAbel Pensky, 33A
 17.6 °FAbel Pensky, 33B
 
Processing PropertiesOriginal ValueComments
Pot Life 5760 - 10080 min(4-7 days) Combined
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceClear to Amber Liquid33A
 Clear to Amber Liquid33B
Typical Coverage1225-1425 ft2/US gal
VOC0.5733A
 0.7833B

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBCHEM026 / 317445

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.