MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC XENOY X5100 PC+Polyester (Europe-Africa-Middle East)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polyester, TP

Material Notes: XENOY X5100 is a semi-crystalline, impact modified PC-PBT blend with excellent flow. (PC+PBT-I).

Information provided by SABIC Innovative Plastics for Europe-Africa-Middle East.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
Moisture Absorption 0.150 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.50 %
@Temperature 23.0 °C
ISO 62
Viscosity 215000 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
Melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0070 - 0.010 cm/cmon Tensile Bar; SABIC Method
Melt Flow 13 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 40.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 54.0 MPa50 mm/min; ISO 527
Elongation at Break 50 %50 mm/min; ISO 527
Elongation at Yield 4.5 %50 mm/min; ISO 527
Tensile Modulus 2150 MPa1 mm/min; ISO 527
Flexural Yield Strength 80.0 MPa2 mm/min; ISO 178
Flexural Modulus 2050 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 18.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
 20.0 kJ/m²
@Temperature -20.0 °C
80*10*4; ISO 180/1A
 35.0 kJ/m²
@Temperature -10.0 °C
80*10*4; ISO 180/1A
 40.0 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
 45.0 kJ/m²
@Temperature 23.0 °C
80*10*4; ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 15.0 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 40.0 kJ/m²
@Temperature 0.000 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
 50.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 85.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KISO 8302
Hot Ball Pressure Test 75.0 °CPass; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 105 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Deflection Temperature at 1.8 MPa (264 psi) 84.0 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
Vicat Softening Point 117 °CRate B/50; ISO 306
 120 °CRate B/120; ISO 306
 135 °CRate A/50; ISO 306

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI49682 / 190767

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.