MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
PolyPLASTY PolyJARID PA 6 G Polyamide 6 cast, Dry
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, Unreinforced

Material Notes:
  • Polyamide casted: Semi-products and parts weighing up to 2 tons
  • Machined parts: Turned and milled parts in single and serial production

Information provided by PolyPLASTY.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Absorption 2.8 %under regular conditions; ISO 62
Moisture Absorption at Equilibrium 8.0 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, H358/30 160 MPaISO 2039-1
Tensile Strength, Yield 90.0 MPaISO 527
Elongation at Break 20 %ISO 527
Modulus of Elasticity 3.60 GPaISO 527
Flexural Strength 140 MPaISO 178
Izod Impact, Notched (ISO) 7.00 kJ/m²ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature 23.0 °C
ISO 180/1C
 NB
@Temperature -30.0 °C
ISO 180/1C
Tensile Creep Modulus, 1000 hours 2300 MPa0.5 percent; ISO 899-1
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 1.00e+13 ohm-cmIEC 60093
Surface Resistance 1.00e+12 ohmIEC 60093
Dielectric Constant 3.7
@Frequency 1e+6 Hz
IEC 60250
Dielectric Strength 100 kV/mm
@Thickness 0.600 mm
IEC 60243-1
Dissipation Factor 0.030
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 600 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Transverse to Flow 80.0 µm/m-°CISO 11359
Specific Heat Capacity 1.68 J/g-°CIEC 1006
Thermal Conductivity 0.290 W/m-KDIN 52 612
Melting Point 220 °C
Maximum Service Temperature, Air 80.0 °Clong term
 150 °Cshort term
Deflection Temperature at 0.46 MPa (66 psi) 120 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 185 °CISO 75
Vicat Softening Point 215 °C
@Load 5.10 kg
point B; ISO 306 VST/B/50
Minimum Service Temperature, Air -40.0 °C
Flammability, UL94 V-2
@Thickness 3.20 mm
IEC 60695-11-10
 
Descriptive Properties
LOI Acid Index (%)25ISO 4589

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Overview of materials for Nylon 66, 10% Glass Fiber Filled
Overview of materials for ECTFE Fluoropolymer
Covestro Desmopan® 790 Polyurethane
3D Systems QuickPlastic Cast Urethane Material GlassFilled Nylon

PPOLYPL923 / 197633

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.