Hostacom TRC 411N R is a 20% talc filled PP copolymer compound, with high flowability, good impact/stiffness balance and excellent scratch resistance, offering low odor and low emissions performances. This polypropylene compound is produced locally in Russia. The grade being in development, this is a preliminary datasheet subjected to changes after product industrialization. Applications : Automotive Parts, Instrument Panels, Interior Automotive Applications. |