Polypropylene copolymer, 20% talcum filled, flame retardant UL94 V0, designed according to RoHS Decree. Available: all colors, UV stabilized (L), heat stabilized (S), laser printable (YT), detergent stabilized (D).Information provided by Taro Plast S.p.a. |