MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Stratasys® VeroYellowV Rigid Opaque 3D Printing Polymer
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer

Material Notes: This multi-purpose material is most widely used for visual models, engineering prototypes, product assemblies and RTV molding patterns. Rigid Opaque materials are good material choices for light functional testing, patterns, prototypes and models. Available in seven hues including blue, white, black, gray, cyan, magenta and yellow, the Vero family shares similar mechanical, thermal and electrical properties. The medium shades of VeroBlue™ and VeroGray™ provide the best detail visualization, without glare or darkness. The VeroVivid™ family of VeroCyanV™, VeroMagentaV™ and VeroYellowV™ offers more saturated and vibrant color. Vero PureWhite™ is twice as opaque, 20 percent brighter and more UV resistant than VeroWhitePlus™.

Information provided by Stratasys.

Vendors:
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.17 - 1.18 g/ccPolymerized
Water Absorption 1.1 - 1.5 %
@Time 86400 sec
D-570-98
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell M 73 - 76
Hardness, Shore D 83 - 86
Tensile Strength 50.0 - 65.0 MPaD-638-03
Elongation at Break 10 - 25 %D-638-05
Modulus of Elasticity 2.00 - 3.00 GPaD-638-04
Flexural Strength 75.0 - 110 MPaD-790-03
Flexural Modulus 2.20 - 3.20 GPaD-790-04
Izod Impact, Notched 20.0 - 30.0 J/mD-256-06
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 45.0 - 50.0 °CD-648-06
Deflection Temperature at 1.8 MPa (264 psi) 45.0 - 50.0 °CD-648-07
Glass Transition Temp, Tg 52.0 - 54.0 °CDMA, E»

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSTRAS938 / 255820

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.