MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ITW Chockfast® Blue Epoxy Grouting Compound
Categories: Polymer; Thermoset; Epoxy

Material Notes: CHOCKFAST Blue is a two-component, aggregate-filled, pourable epoxy grouting compound for severe applications. This highly developed material is often used to replace steel soleplates or rails and is used as an epoxy foundation capping material that is resistant to high operating temperatures. Its unique properties permit usage directly under highly stressed machinery mounting surfaces.

USE & BENEFITS: Typical applications include the grouting of diesel engines, compressors, generators, gears, pumps and most other heavy equipment. CHOCKFAST Blue is best in class under heavy reciprocating and rotary machinery due to its excellent resistance to creep, fatigue and shock forces. It is also an excellent support surface for the CHOCKFAST Black epoxy chock.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.00 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3156 psiASTM D640
Flexural Strength 4920 psiASTM C580
Flexural Modulus 1.70e+6 psiASTM C580
Compressive Strength 19000 psiASTM C579 MOD
Compressive Modulus 1.64e+6 psiASTM C579 MOD
Izod Impact, Notched 0.280 ft-lb/inASTM D258
 
Thermal PropertiesOriginal ValueComments
CTE, linear 15.4 µin/in-°F
@Temperature 0.000 - 60.0 °C
ASTM D696
Shrinkage 0.010 %Linear; ASTM D2566
 
Processing PropertiesOriginal ValueComments
Cure Time 11.0 hour
@Temperature 32.0 °C
approximate
 16.0 hour
@Temperature 27.0 °C
approximate
 24.0 hour
@Temperature 21.0 °C
approximate
 36.0 hour
@Temperature 16.0 °C
approximate
Pot Life 35.0 - 50.0 min
@Temperature 21.1 °C
 
Descriptive Properties
Fire Resistanceself extinguishingASTM D637

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWC9026 / 239536

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.