System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Petropol Petrotene® A3 G30 DOR0078 PH328 PP, 30% Glass Fiber Reinforced
Categories:
Polymer
;
Thermoplastic
;
Polypropylene (PP)
;
Polypropylene with 30% Glass Fiber Filler
Material Notes:
Polypropylene homopolymer in golden color reinforced with 30% glass fiber suitable for injection molding, good set mechanical properties, aging resistance and excellent resistance to oils and greases.
Information provided by Petropol
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Density
1.10
-
1.13
g/cc
0.0397
-
0.0408
lb/in³
ASTM D792
Water Absorption
0.030 %
0.030 %
Humidity Absorption; ASTM D570
Linear Mold Shrinkage
0.0040
-
0.0080
cm/cm
0.0040
-
0.0080
in/in
ASTM D955
Melt Flow
15
-
20
g/10 min
15
-
20
g/10 min
ASTM D1238
Ash
28 - 32 %
28 - 32 %
ASTM D2584
Mechanical Properties
Metric
English
Comments
Hardness, Rockwell R
90
90
Tensile Strength
55.0
MPa
7980
psi
ASTM D638
Elongation at Break
10 %
10 %
ASTM D638
Flexural Strength
95.0
MPa
13800
psi
ASTM D790
Flexural Modulus
4.00
GPa
580
ksi
ASTM D790
Izod Impact, Notched
0.760
J/cm
1.42
ft-lb/in
ASTM D256
Electrical Properties
Metric
English
Comments
Dielectric Strength
40.0
kV/mm
1020
kV/in
ASTM D257
Dissipation Factor
0.0010
@Frequency 1000 Hz
0.0010
@Frequency 1000 Hz
ASTM D150
Thermal Properties
Metric
English
Comments
Deflection Temperature at 1.8 MPa (264 psi)
120
°C
248
°F
2ºC/min; ASTM D696
Vicat Softening Point
145
°C
293
°F
ASTM D1525A
Flammability, UL94
HB
HB
Processing Properties
Metric
English
Comments
Processing Temperature
190
-
230
°C
374
-
446
°F
Molding
Mold Temperature
60.0
-
80.0
°C
140
-
176
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
hour
2.00
hour
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
PPETROPOL275 / 313183
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.