MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials TIVAR® 1000 EC Electrically Conductive UHMW-PE (ASTM Product Data Sheet)
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes:

Quadrant Engineering Plastic Products is now Mitsubishi Chemical Advanced Materials.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.940 g/ccASTM D792
Water Absorption <= 0.010 %Immersion, 24hr; ASTM D570(2)
Water Absorption at Saturation <= 0.010 %Immersion; ASTM D570(2)
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 66ASTM D2240
Tensile Strength 5800 psiASTM D638
Tensile Strength at 65°C (150°F) 400 psiASTM D638
Elongation at Break 300 %ASTM D638
Tensile Modulus 101 ksiASTM D638
Flexural Strength 3200 psiASTM D790
Flexural Modulus 101 ksiASTM D790
Compressive Strength 3300 psi10% Def.; ASTM D695
Compressive Modulus 100000 psiASTM D695
Izod Impact, Notched NBASTM D256 Type A
Coefficient of Friction, Dynamic 0.12Dry vs. Steel; QTM55007
Sand Slurry 101018 Steel = 100
Limiting Pressure Velocity 3000 psi-ft/min4:1 safety factor; QTM 55007
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square <= 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear 110 µin/in-°F
@Temperature -40.0 - 149 °C
ASTM E831
Melting Point 260 °FCrystalline, Peak; ASTM D3418
Maximum Service Temperature, Air 180 °FLong Term
Deflection Temperature at 1.8 MPa (264 psi) 116 °FASTM D648
Flammability, UL94 HB
@Thickness 3.17 mm
Estimated Rating
 
Compliance PropertiesOriginal ValueComments
3A-Dairy No
Canada AG No
FDA No
NSF No
USDA No
USP Class VI No
 
Chemical Resistance PropertiesOriginal ValueComments
Acids, Strong (pH 1-3) Limited
Acids, Weak Acceptable
Alcohols Acceptable
Alkalies, Strong (pH 11-14) Acceptable
Alkalies, Weak Acceptable
Chlorinated Solvents Acceptable
Conductive / Static Dissipative Yes
Continuous Sunlight Limited
Hot Water / Steam Limited
Hydrocarbons - Aliphatic Acceptable
Hydrocarbons - Aromatic Unacceptable
Inorganic Salt Solutions Acceptable
Ketones, Esters Limited
 
Descriptive Properties
ColorBlack
Machinability31-10, 1=Easier to Machine

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mitsubishi Chemical Advanced Materials TIVAR® 1000 UHMW-PE, (Natural & Colors except Black) (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 1000 antistatic UHMW-PE / TIVAR® ESD UHMW-PE (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® DrySlide UHMW-PE, Lubricant Filled, Electro Static Dissipative, UV Stabilized (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® UV Stabilized UHMW-PE, Black (ASTM Product Data Sheet)
Mitsubishi Chemical Advanced Materials TIVAR® 1000 ASTL UHMW-PE + specific additives (ISO Data)

P1SMP04 / 20153

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.