MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LEXAN LUX7630C PC Copolymer (Americas)  (Unverified Data**)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LEXAN LUX7630C Polycarbonate (PC) resin is a non-filled resin, suitable for injection molding and extrusion. This non-chlorinated, non-brominated flame retardant PC has an UL-94 V0 rating at 1.0 mm / 5VA rating at 3.0mm and is UV stabilized (F1 rating) providing additional weathering capability. LEXAN LUX7630C is available in transparent natural colors only.

Information provided by SABIC Innovative Plastics for the Americas.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.19 g/ccASTM D 792
Density 1.20 g/ccISO 1183
Moisture Absorption 0.110 %
@Temperature 23.0 °C
50% RH; ISO 62
Water Absorption at Saturation 0.14 %
@Temperature 23.0 °C
ISO 62
Linear Mold Shrinkage, Flow 0.0055 - 0.0075 cm/cm
@Thickness 3.20 mm
SABIC Method
Linear Mold Shrinkage, Transverse 0.0060 - 0.0080 cm/cm
@Thickness 3.20 mm
SABIC Method
Melt Flow 5.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
cm^3/10 min Melt Volume Rate; ISO 1133
 5.0 g/10 min
@Load 1.20 kg,
Temperature 300 °C
ASTM D 1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 52.0 MPa50 mm/min; ISO 527
 52.0 MPaType I, 50 mm/min; ASTM D 638
Tensile Strength, Yield 67.0 MPa50 mm/min; ISO 527
 68.0 MPaType I, 50 mm/min; ASTM D 638
Elongation at Break 23 %50 mm/min; ISO 527
 51 %Type I, 50 mm/min; ASTM D 638
Elongation at Yield 6.0 %50 mm/min; ISO 527
 6.0 %Type I, 50 mm/min; ASTM D 638
Tensile Modulus 2400 MPa1 mm/min; ISO 527
 2500 MPa50 mm/min; ASTM D 638
Flexural Yield Strength 103 MPa2 mm/min; ISO 178
 106 MPa1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 2400 MPa1.3 mm/min, 50 mm span; ASTM D 790
 2500 MPa2 mm/min; ISO 178
Izod Impact, Notched 85.0 J/m
@Temperature -30.0 °C
ASTM D 256
 100 J/m
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched NB
@Temperature -30.0 °C
ASTM D 4812
 NB
@Temperature 23.0 °C
ASTM D 4812
Izod Impact, Notched (ISO) 9.00 kJ/m²
@Temperature -30.0 °C
80*10*3; ISO 180/1A
 10.0 kJ/m²
@Temperature 23.0 °C
80*10*3; ISO 180/1A
Izod Impact, Unnotched (ISO) NB
@Temperature -30.0 °C
80*10*3; ISO 180/1U
 NB
@Temperature 23.0 °C
80*10*3; ISO 180/1U
Charpy Impact Unnotched NB
@Temperature -30.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
 NB
@Temperature 23.0 °C
Edgew 80*10*3 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
V-notch Edgew 80*10*3 sp=62mm; ISO 179/1eA
Instrumented Impact Total Energy 66.0 J
@Temperature 23.0 °C
ASTM D 3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.79
@Frequency 1.10e+9 Hz
ASTM ES 7-83
Dissipation Factor 0.0058
@Frequency 1.10e+9 Hz
ASTM ES 7-83
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 66.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 72.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 70.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E 831
 76.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 131 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 131 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Deflection Temperature at 1.8 MPa (264 psi) 120 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 120 °C
@Thickness 3.20 mm
unannealed; ASTM D 648
Vicat Softening Point 136 °CRate B/50; ASTM D 1525
 137 °CRate B/50; ISO 306
 139 °CRate B/120; ISO 306
UL RTI, Electrical 125 °CUL 746B
UL RTI, Mechanical with Impact 120 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 V-2
@Thickness 0.400 mm
UL 94
 V-0
@Thickness 1.00 mm
UL 94
 5VA
@Thickness 3.00 mm
UL 94
Oxygen Index 45 %ISO 4589
Glow Wire Ignition Temperature 875 °C
@Thickness 1.00 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 1.00 mm
IEC 60695-2-12
 
Optical PropertiesOriginal ValueComments
Transmission, Visible >= 91 %ASTM D 1003
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

**
This data sheet is not an active part of MatWeb and the information on it should not be considered reliable.
Inactive data sheets have usually been replaced with newer information on the same material. If this is the case, you can find the active data sheet by using any of our search tools, including the Quick Search box in the upper part of this page.
If you are unable to locate an active data sheet for this material, then this material is likely discontinued, although various other reasons may be behind its removal. In any event, do not rely on the information on this page to be accurate or maintained.
You may have reached this data sheet through an outdated bookmark or link. Please update your bookmark accordingly. We apologize if you have accessed this page through MatWeb’s usual search tools.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultrason® E 2010 PES
BASF Ultrason® E 3010 PES
INEOS Styrolution Luran® S KR 2863 C UV Colored ASA+PC
Resistalloy International Resistalloy 8020 Nickel Chromium Electrical Resistance Alloy
SABIC ULTEM 1100V PEI

PSABI46301 / 187386

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.