MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Epoxies, Etc UV CURE 60-7156 Flexible UV Curable Adhesive & Potting Compound
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: Description: UV Cure 60-7156 is a one- component epoxy that cures with low intensity black light or high intensity UV lamps. UV 60-7156 is water clear and is designed to be used as an adhesive, coating, or encapsulant. This system is moisture and chemical resistant. Its low durometer (flexibility) provides less stress on sensitive electronic components. UV Cure 60-7156 is a good choice for potting and encapsulating applications due to its ability to deep section cure up to ¾ inch. Another unique and important feature is its ability to “dark cure.” Once exposed to UV light the UV Cure 60-7156 will continue to cure in the absence of light. This is advantageous when potting or joining substrates with shadow areas. UV Cure 60-7156 may also be heat cured as a secondary cure operation. UV Cure 60-7156 is not affected by oxygen and will not have a sticky or greasy surface. The surface is flexible, smooth, and glossy when properly cured. UV Cure 7156 bonds to metal, plastic, paper and ceramic.

Features:

  • One component
  • Excellent adhesion
  • Contains no solvents
  • Good electrical insulation
  • Low shrinkage
  • No out gassing
  • Will shadow cure
  • Good weathering resistance
  • Cure is not inhibited by oxygen
  • Low odor

Information provided by Epoxies, Etc

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.09 g/cc
Solids Content 100 %
Viscosity 600 cP
Storage Temperature 4.40 - 15.6 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 95
Tensile Strength 6200 psi
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 425 V/mil
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 200 °C
Minimum Service Temperature, Air -50.0 °C
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
 
Descriptive Properties
ColorWater clear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PFEPOX101 / 316778

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.