MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
HB Fuller 1536 Silicone sealant
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: 1536 is grey, flowable, one-component, neutral alkoxy-cure silicone sealant. Low-odor, solvent-free, cure at room temperature when exposed to moisture at the atmosphere. With fast tack free time and meets UL94-V0 flame rating. Excellent adhesion to glass, ABS, FR4, and PCBs. Superior resistance to thermal cycling, damp-heat, and damp-freezing. Typical applications include electronics encapsulation, connector staking, electronics potting, circuit board encapsulation, electrical component re-enforcement, electronic component bonding, and sealing.

Features and Benefits:

  • Meets UL94-V0 flame rating
  • Excellent heat resistance properties
  • Excellent thermal cycle, damp heat and damp freezing performance.
  • Easy to use for reworkable applications
  • Very good electrical insulation properties
  • Neutral cure low/no odor
Typical Applications:
  • Electrical insulation
  • Protects leads from mechanical shock
  • Bond and seal enclosures
  • Seals ductwork, vents, flues, doors, windows
  • Sealing and waterproofing for transformer

Information provided by H.B. Fuller Company

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.21 g/cc
Viscosity 15000 - 30000 cP
Storage Temperature 5.00 - 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35ISO 7619
Tensile Strength 1.50 MPaISO 37
Elongation at Break 150 %ISO 37
Shear Strength 0.500 MPaISO 4587
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmIEC 60093
Dielectric Strength 15.0 kV/mmIEC 60243-1
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 210 °C
Minimum Service Temperature, Air -54.0 °C
 
Processing PropertiesOriginal ValueComments
Cure Time 5.00 - 20.0 minTack Free Time
 24.0 hour
@Thickness >=2.00 mm
Full Cure
 
Descriptive Properties
ColorGrey
ConsistencyLiquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PHBFULL107 / 316898

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.