MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound DX09301C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX09301C compound is based on Polycarbonate (PC) resin containing conductive carbon powder. Added features of this grade include: LNP Clean Compounding Technology, Low LPC, Low Ionics, Low Outgassing, Electrically Conductive.

Features: LNP Clean Compound Technology,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.22 g/ccISO 1183
 1.224 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
Linear Mold Shrinkage, Flow 0.0050 - 0.0070 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0050 - 0.0070 cm/cm24hrs; ASTM D955
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 51.0 MPa5 mm/min; ASTM D638
 54.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 64.0 MPa5 mm/min; ASTM D638
 66.0 MPa5 mm/min; ISO 527
Elongation at Break 12 %5 mm/min; ISO 527
 15 %5 mm/min; ASTM D638
Elongation at Yield 3.1 %5 mm/min; ISO 527
 5.4 %5 mm/min; ASTM D638
Tensile Modulus 2600 MPa1 mm/min; ISO 527
 2670 MPa50 mm/min; ASTM D638
Flexural Strength 99.0 MPayield, 2 mm/min; ISO 178
 101 MPabrk, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2560 MPa2 mm/min; ISO 178
 2600 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 52.0 JASTM D256
Izod Impact, Unnotched 2160 J/mASTM D4812
Izod Impact, Notched (ISO) 4.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 200 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 8.00 Jpeak; ASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1000 - 1.00e+7 ohm-cmASTM D257
Surface Resistance 1000 - 1.00e+7 ohmASTM D257
Static Decay <= 0.10 sec5000V to <50V; FTMS101B
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) 126 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81259 / 289206

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.