MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Celanese Rynite® 530 BK503 PET-GF30
Categories: Polymer; Thermoplastic; Polyester, TP; Polyethylene Terephthalate (PET); Polyethylene Terephthalate (PET), 30% Glass Reinforced

Material Notes: 30% Glass Reinforced Polyethylene Terephthalate

Former DuPont product acquired by Celanese in 2022.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.56 g/ccISO 1183
Water Absorption 0.050 %
@Time 86400 sec
Immersion; Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0030 cm/cmISO 294-4, 2577
 0.0010 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
Postmolding shrinkage; ISO 294-4
Linear Mold Shrinkage, Transverse 0.0090 cm/cmISO 294-4, 2577
 0.0045 cm/cm
@Treatment Temp. 80.0 °C,
Time 173000 sec
Postmolding shrinkage; ISO 294-4
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 120ISO 2039-2
Ball Indentation Hardness 221 MPaH 961/30; ISO 2039-1
Tensile Strength at Break 150 MPaISO 527-1/-2
Elongation at Break 2.1 %ISO 527-1/-2
Tensile Modulus 10200 MPaISO 527-1/-2
Flexural Strength 210 MPaISO 178
Flexural Modulus 8940 MPaISO 178
Compressive Strength 230 MPaISO 604
Poissons Ratio 0.34
Izod Impact, Notched (ISO) 8.50 kJ/m²
@Temperature -40.0 °C
ISO 180/1A
 9.50 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Izod Impact, Unnotched (ISO) 35.0 kJ/m²
@Temperature -40.0 °C
ISO 180/1U
 45.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1U
Charpy Impact Unnotched 45.0 kJ/m²
@Temperature -40.0 °C
ISO 179/1eU
 52.0 kJ/m²
@Temperature 23.0 °C
ISO 179/1eU
Charpy Impact, Notched 8.00 kJ/m²
@Temperature -40.0 °C
ISO 179/1eA
 8.50 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 9.50 kJ/m²
@Temperature 23.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Surface Resistance >= 1.00e+15 ohmIEC 62631-3-2
Dielectric Constant 4.2
@Frequency 1e+6 Hz
IEC 62631-2-1
 4.5
@Frequency 100 Hz
IEC 62631-2-1
Dielectric Strength 32.0 kV/mmIEC 60243-1
Dissipation Factor 0.0152
@Frequency 1e+6 Hz
IEC 62631-2-1
 0.031
@Frequency 100 Hz
IEC 62631-2-1
Comparative Tracking Index 250 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.290 W/m-KSolid
Melting Point 250 °C10°C/min; ISO 11357-1/-3
Deflection Temperature at 0.46 MPa (66 psi) 244 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 221 °CISO 75-1/-2
Glass Transition Temp, Tg 90.0 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HB
@Thickness 0.810 mm
IEC 60695-11-10
 HB
@Thickness 1.50 mm
IEC 60695-11-10
Flame Spread 38.0 mm/min
@Thickness 1.00 mm
ISO 3795 (FMVSS 302)
 
Processing PropertiesOriginal ValueComments
Melt Temperature 285 °COptimum, Injection
 280 - 300 °CRange, Injection
Mold Temperature 120 °COptimum, Injection
 110 - 130 °CInjection
Ejection Temperature 170 °CInjection
Drying Temperature 120 °CInjection
Dry Time 4.00 - 6.00 hourInjection, Dehumidified Dryer
Moisture Content <= 0.020 %Injection
Hold Pressure >= 80.0 MPaInjection
 
Descriptive Properties
Back pressureAs low as possible
Drying RecommendedyesInjection
Emission of organic compounds (µgC/g)16VDA 277
FMVSS ClassBISO 3795 (FMVSS 302)
Fogging (mg)0G-value (condensate); ISO 6452
Max. screw tangential speed (m/s)0.2Injection
Odor Class3VDA 270
Part Marking Code>PET-GF30<ISO 11469
PolymerPET-GF30
Processing Hold Pressure Time (s/mm)4Injection
Resin IdentificationPET-GF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Covestro Makrolon® Rx1805 Polycarbonate
Elektro-Isola G-Etronax EP FR4 Epoxy, Glass Fabric Reinforcement, Light Yellow, Sheets
Celanese Rynite® 530 NC010 PET-GF30
Covestro Makrolon® 9417 Polycarbonate, 10% Glass Filled
Polymer Resources PPX-FR4 Modified-PPO, V-1 Flame Retardant

PDSX5258 / 197898

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.