MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Danquinsa DANTHANE® 125K-20F Powder Coating
Categories: Polymer; Thermoplastic; Adhesives, Sealants, and Coatings

Material Notes: The TPU compound DANTHANE_ 125K-20F Powder is a special compound powder based on TPU/PTFE. This type is specially suitable for sinter coating of technical textiles. DANTHANE_ 125K-20F-Powder can also be used for dot point and double dot point coating. This compound powder combines the properties of high flexibility of a TPU together with the excellent chemical non-stick properties of Teflon (polytetrafluorethene PTFE). DANTHANE_ 125K- 20F-Powder is mainly used for the coating of transport elements and conveyor belts, drive sections (flat drive belts) and for the coating of materials for big-bags, materials for containers and for special hoses. Beside the properties of TPU coatings, the advantage of DANTHANE_ 125K-20F-Powder is the high resistance against contamination and the very high slippage of the surface. So laminated materials are self-cleaning because at pure TPU-coatings contaminations can set down more easy than at coatings made with DANTHANE_ 125K-20F-Powder.

Application: DANTHANE_ 125K-20F Powder is processed by sinter coating, dot point coating and double dot point coating for coatings of industrial textiles. For sinter coating this product will be delivered with a grit size of 50 – 500µ. The special grit sizes of DANTHANE_ 125K-20F-Powder are also suitable for the impregnations of textiles. DANTHANE_ 125K-20F-Powder is mainly used for the coating of textile and non-woven supporting materials. It can be applied as medium layer as well as top coat. Due to the good slip and surface properties, DANTHANE_ 125K-20F-Powder is mainly used as top coat. As medium layer it could be combined the classical types DANTHANE_ 125KPowder respectively DANTHANE_ 126K-Powder. Concerning impregnation and primers of the corresponding textiles and other supporting materials we refer to the primers of the DANCOLL_ range.

Information provided by Danquinsa GMBH

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccDIN 53.479
Melt Flow 65 - 95 g/10 min
@Load 10.0 kg,
Temperature 190 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 86DIN 53.505
Tensile Strength 30.0 MPaDIN 53.504
Elongation at Break 500 %DIN 53.504
100% Modulus 5.50 MPaDIN 53.504
200% Modulus 6.00 MPaDIN 53.504
300% Modulus 8.50 MPaDIN 53.504
Abrasion 20[mm³]; DIN 53.516
Compression Set 30 %
@Temperature 23.0 °C,
Time 252000 sec
DIN 53.517
 80 %
@Temperature 70.0 °C,
Time 86400 sec
DIN 53.517
 
Thermal PropertiesOriginal ValueComments
Melting Point 140 - 145 °CKofler
Softening Point 135 - 140 °CKofler
 140 - 145 °CCharacteristic of the film
Glass Transition Temp, Tg -27.0 °CDSC; DIN 51.007
 
Processing PropertiesOriginal ValueComments
Shelf Life 6.00 Month
 
Descriptive Properties
AspectWhite colored pearl granule(RAL 9011)
 white, elasticCharacteristic of the film

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PDANQ137 / 294557

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.