Compound 8748 is a 70 durometer black colored Viton that is formulated with FDA approved materials. It exhibits excellent resistance to heat, petroleum based oils, aliphatic and aromatic fuels. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 2 HK 715 A1-10 B37 B38 EF31 EO78; 4 HK 715 A1-11 B38 EF31 EO78; 6 HK 715 A1-10 A1-11 B31 B38 EF31 EO88 3-A Sanitary Standards 18-03 Class I, II, III & IV Information provided by Pressure Seals Inc. |