MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lubrizol Advanced Materials Stat-Rite® S-403 Olefin Block Copolymer
Categories: Polymer; Thermoplastic; Elastomer, TPE; Olefinic TPE

Material Notes: Product Description: S-403 is a transparent, static dissipative olefin co-polymer alloy. It utilizes the patented Stat-Rite® inherently static dissipative polymer (IDP) to provide clean, permanent ESD protection. Stat-Rite® IDP alloys provide consistent static dissipation even when extruded, injection molded or thermoformed into components. Features: Transparent; Permanent static dissipative performance; Ultra-clean: low off-gassing, low ionic contamination; No particulate fillers; Durable: Can be used for years and years. Applications: Photomask packaging; Wafer carriers/pad; Optical films; Machine/equipment site glass; Sample shipping boxes
Availability: Asia Pacific, Europe, Latin America, North America
Features: Antistatic; Clean/High Purity; Durable; ESD Protection; Low (to None) Ion Content; Low to No Outgassing; Rapid Static Decay
Uses: Film; Optical Applications; Packaging
Appearance: Clear/Transparent
Forms: Pellets
Processing Method: Extrusion; Injection Molding; Thermoforming

Information provided by Lubrizol Advanced Materials, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.06 g/ccASTM D792
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Yield 5810 psiASTM D638
Elongation at Break 40 %ASTM D638
Tensile Modulus 270000 psiASTM D638
Flexural Modulus 265000 psiASTM D790
Izod Impact, Notched 2.00 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 2.00e+10 ohm-cmASTM D257
Surface Resistance 1.00e+9 ohm12% RH; ESD S11.11
Surface Resistivity per Square 1.00e+10 ohm50% RH; ASTM D257
Static Decay <= 2.0 sec1000 V to 100 V, CPM, 50% RH
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 156 °FUnannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 138 °FUnannealed; ASTM D648
 
Descriptive Properties
Ionic Content1 ng/gCation Mg+
 10 ng/gAnions SO4, Test Method #3010-4
 15 ng/gAnion Cl , Test Method #3010-4
 15 ng/gAnions NO3, Test Method #3010-4
 25 ng/gCation Na+
 3 ng/gAnion F, Test Method #3010-4
 3 ng/gCation K+
 40 ng/gCation Li+
 5 ng/gCation NH4+
 60 ng/gAnions PO4, Test Method #3010-4
 85 ng/gCation Ca+
Outgassing<0.02 µg/gStyrene , Test Method #3010-3
 <0.02 µg/gToluene , Test Method #3010-3
 <0.03 µg/gMMA , Test Method #3010-3
 1.5 µg/gTotal Organics , Test Method #3010-3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLUBR6023 / 268325

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.