MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Syensqo (Solvay Specialty Polymers) Xydar® M-345 LCP, 45% mineral filled
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), Mineral Filled

Material Notes: 45% mineral filled, SMT processing

Xydar® M-345 liquid crystal polymer (LCP) is a 45% mineral reinforced injection molding grade developed for electrical/electronic applications utilizing surface mount technology. The material can fill very thin walls over long flow lengths.

In addition to low warpage, it exhibits good strength and stiffness (even at elevated temperatures), low coefficient of thermal expansion, high heat deflection temperature, inherent flame resistance and good chemical and weathering resistance.

- Natural: M-345 NT
- Black: M-345 BK

Features: Chemical Resistant; Flame Retardant; Good Moldability; Good Stiffness; Good Strength; Good Weather Resistance; Low Warpage

Information provided by Solvay Specialty Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.80 g/ccISO 1183
Ash 45 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 80.0 MPaISO 527-2
Elongation at Break 2.5 %ISO 527-2
Tensile Modulus 8200 MPaChord; ISO 527-2
Flexural Strength 87.0 MPaASTM D790
Flexural Modulus 9700 MPaChord; ISO 178
Charpy Impact Unnotched 36.0 kJ/m²Complete Break; ISO 179
Charpy Impact, Notched 5.80 kJ/m²Complete Break; ISO 179
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 281 °CUnannealed; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 237 °CUnannealed; ISO 75-2/A
 
Processing PropertiesOriginal ValueComments
Melt Temperature 340 - 370 °CInjection
Mold Temperature 70.0 - 160 °C
Drying Temperature 150 °C
@Time 21600 - 28800 sec
Clamp Pressure 28.0 - 55.0 MPa
 
Descriptive Properties
AvailabilityAsia Pacific
 Europe
 North America
ColorBlack; Natural Color
FormsPellets
ProcessingInjection Molding
Screw Compression Ratio2.5:1.0 to 3.0:1.0
Screw L/D Ratio, Injection20.0:1.0 to 24.0:1.0

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSOL8Y4635 / 280435

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.