MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Arla PC FROST™ PC Sheet
Categories: Polymer; Thermoplastic; Polycarbonate (PC); Polycarbonate, Extruded

Material Notes: PC FROST™ is a transparent polycarbonate sheet. The product is produced by a production team experienced in producing mono, co and tri-extrusion. The product is virtually unbreakable with extremely high impact resistance and offers high temperature performance too. PC FROST™ provides designers, specifiers and architects with possibilities to use FROSTED polycarbonate sheets in applications where a modern and stylish look is required. The consistent high quality demands from the market helps to improve machining and thermoformability.

Benefits: Wide range of transparent colors; More than 10 times the impact strength of high impact PMMA; Easy to thermoform or fabricate; Half the weight of glass

Application: Interior design, signs, displays and in other applications where a high impact strength, good aesthetics and a stylish look are needed.

Information provided by Arla Plast.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.20 g/ccISO 1183
Moisture Absorption 0.150 %
@Time 86400 sec
50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 70.0 MPaISO 527
Tensile Strength, Yield 60.0 MPaISO 527
Elongation at Break 110 %ISO 527
Elongation at Yield 6.0 %ISO 527
Modulus of Elasticity >= 2.30 GPaISO 527
Flexural Modulus >= 2300 MPaISO 178
Izod Impact, Notched (ISO) 10.0 kJ/m²
@Temperature -30.0 °C
ISO 180/1A
 65.0 kJ/m²
@Temperature 23.0 °C
ISO 180/1A
Charpy Impact Unnotched NB
@Temperature -40.0 °C
ISO 179/1eU
Charpy Impact, Notched 11.0 kJ/m²
@Temperature -30.0 °C
ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+14 ohm-cmdry; IEC 60093
Surface Resistance 1.00e+16 ohmdry; IEC 60093
Dielectric Constant 2.9
@Frequency 1e+6 Hz
dry; IEC 60250
 3.0
@Frequency 50 Hz
dry; IEC 60250
Dielectric Strength 30.0 kV/mmdry; IEC 60243
Dissipation Factor 0.0010
@Frequency 50 Hz
(tan d), dry; IEC 60250
 0.010
@Frequency 1e+6 Hz
(tan d), dry; IEC 60250
 
Thermal PropertiesOriginal ValueComments
CTE, linear 65.0 µm/m-°C
@Temperature 20.0 - 70.0 °C
ISO 11359-2
Thermal Conductivity 0.200 W/m-KDIN 8302
Deflection Temperature at 0.46 MPa (66 psi) 142 °CISO 75
Deflection Temperature at 1.8 MPa (264 psi) 132 °CISO 75
Vicat Softening Point 148 °CB 50; ISO 306
 149 °CB 120; ISO 306
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.586ISO 489

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PARLA938 / 301116

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.