MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Lord Adhesives 7433 Urethane Adhesive System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD® 7433 adhesive is a single-component, moisture-cure urethane adhesive used in hose manufacturing to produce high-strength bonds between common reinforcement yarns, thermoplastic tubing and thermoplastic protective hose coverings.

Features: blue color allows for easy identification on light colored extruded tubing, as well as on reinforcement yarns. provides a 100% solids formula that contains no solvents; does not require explosion-proof equipment. requires no mixing; requires no ovens or other heat source for curing.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.11 - 1.16 g/cc0.0403 - 0.0420 lb/in³
Solids Content 100 %100 %by weight
Brookfield Viscosity 50000 - 150000 cP
@Temperature 25.0 °C
50000 - 150000 cP
@Temperature 77.0 °F
Brookfield HAT # 5, 5 rpm
 
Thermal PropertiesMetricEnglishComments
Flash Point >= 93.0 °C>= 199 °Fclosed cup
 
Processing PropertiesMetricEnglishComments
Shelf Life 6.00 Month
@Temperature 24.0 °C
6.00 Month
@Temperature 75.2 °F
from shipment date in original, unopened container
 
Descriptive Properties
AppearanceBlue Liquid

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Lubrizol Pearlstick™ 5714 Thermoplastic Polyurethane
Wacker Geniosil® XL 32 Silane
Henkel Loctite® 3102 Acrylic Light Cure Adhesive

PLORD9126 / 232514

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.