65% mineral/glass fiber, for thick-wall parts (>3mm), heat stabilized Amodel® AS-1566 HS resin is a 65% glass and mineral reinforced polyphthalamide (PPA) resin that exhibits a high deflection temperature and high flexural modulus. This grade was designed specifically to be cost effective for most applications requiring high stiffness, good dimensional stability and chemical resistance. Typical applications for Amodel® AS-1566 HS resin include electrical connectors and housings, motor components, pistons, covers, engine parts and transmission components. - Black: AS-1566 HS BK 324 - Black: AS-1566 HS BK 545 - Natural: AS-1566 HS NT Applications: Automotive Applications; Automotive Electronics; Automotive Under the Hood; General Purpose; Housings; Industrial Applications; Industrial Parts; Lawn and Garden Equipment; Machine/Mechanical Parts; Metal Replacement; Power/Other Tools; Thick-walled Parts; Valves/Valve Parts Features: Chemical Resistant; Creep Resistant; Good Dimensional Stability; Good Toughness; Heat Stabilized; High Heat Resistance; High Strength; Low CLTE; Ultra High Stiffness Injection notes: Storage: - Amodel® compounds are shipped in moisture-resistant packages at moisture levels according to specifications. Sealed, undamaged bags should be preferably stored in a dry room at a maximum temperature of 50°C (122°F) and should be protected from possible damage. If only a portion of a package is used, the remaining material should be transferred into a sealable container. It is recommended that Amodel® resins be dried prior to molding following the recommendations found in this datasheet and/or in the Amodel® processing guide. Information provided by Solvay Specialty Polymers. |