MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives 810 Low Read-Through (LRT) Acrylic Adhesive with Accelerator 20GB
Categories: Polymer; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes: LORD® 810 Low Read-Through (LRT) acrylic adhesive when cured with LORD Accelerator 20GB creates a flexible adhesive system for bonding metals, such as aluminum, galvanized steel and CRS, and engineered plastics, such as PC-ABS. LORD 810 adhesive in combination with LORD Accelerator 20GB delivers fast cure speed and strong bonding with minimal bondline read-through (BLRT). LORD Accelerator 20GB allows precise control of the adhesive bondline thickness due to its content of glass beads. LORD 810 adhesive is flammable. Do not store or use near heat, sparks or open flame.

Features: bonds thin and flexible substrates with little to no bondline read-through. requires little or no substrate preparation for bonding metals and plastics. remains in position when applied on vertical or overhead surfaces, allowing for greater process flexibility. resists dilute acids, alkalis, solvents, greases, oils and moisture; provides excellent resistance to indirect UV exposure and weathering. performs at temperatures from -40°F to +300°F (-40°C to +149°C).

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 7.80 - 8.10 lb/gal
Brookfield Viscosity 40000 - 130000 cP
@Temperature 25.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 40Cured
 69Post-Baked
Tensile Strength at Break 5.80 MPaCured
 14.4 MPaPost-Baked
Elongation at Break 22 %Post-Baked
 190 %Cured
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 300 °F
Minimum Service Temperature, Air -40.0 °F
Glass Transition Temp, Tg 43.0 °CCured
 58.0 °CPost-Baked
Flash Point 15.0 °C
 
Processing PropertiesOriginal ValueComments
Pot Life 20.0 - 25.0 min
@Temperature 21.0 °C
Time to Handling Strength, 50 psi shear
Working Life 8.00 - 12.0 min
@Temperature 21.0 °C
 
Descriptive Properties
AppearanceBlack Paste
 GreyCured Appearance
 Grey PasteMixed Appearance
Mix Ratio1.1 to 1by weight, adhesive to accelerator
 2 to 1by volume, adhesive to accelerator

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9110 / 232498

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.