MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ITW Plexus® MA832 Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: Plexus® MA832 is an advanced two-part methacrylate adhesive designed for structural bonding of metals without primers. In addition, MA832 does a superb job of bonding thermoplastic and composite assemblies with little to no surface preparation.  Combined at a 10:1 ratio, MA832 has a working time approximately 14 minutes and achieves approximately 500 psi (3.5 MPa) in 55 minutes. This product provides a unique combination of high strength, excellent fatigue endurance, outstanding impact resistance, and superior toughness. Plexus MA832 is available in gray and is supplied ready-to-use as a non-sagging gel.

Excellent resistance to: ? Hydrocarbons ? Acids and Bases (pH 3-10) ? Salt Solutions.  Susceptible to: ? Polar Solvents ? Strong Acids and Bases.  Recommended for: ? ABS ? Acrylics ?Aluminum ? Epoxies ? FRP ? Gel coats ? PVC ? Polyesters (including DCPD modified) ? Steel (Exterior applications require the use of coatings or primers that inhibit oxidation of the steel.)  ? Styrenics ? Urethanes (general) ? Vinyl Esters.

Adhesive color:  off white, uncured-room temperature.  Activator color:  gray or gray GB, uncured-room temperature.

Information provided by ITW Performance Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.06 lb/galadhesive. Uncured.
 8.17 lb/galCured
 9.10 lb/galActivator. Uncured.
 9.25 lb/galActivator. Uncured.
Volatile Organic Compounds (VOC) Content <= 10 g/lDuring cure
Viscosity 35000 - 80000 cP
@Temperature 22.2 °C
Activator
 80000 - 130000 cP
@Temperature 22.2 °C
Adhesive
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 2700 - 3000 psiASTM D638
Elongation at Break 30 - 60 %ASTM D638
Tensile Modulus 70000 - 100000 psiASTM D638
Adhesive Bond Strength 2000 - 2800 psiLap Shear Cohesive Strength; ASTM D1002
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 180 °F
Minimum Service Temperature, Air -40.0 °F
Flash Point 51.0 °F
 
Processing PropertiesOriginal ValueComments
Working Life 12.0 - 16.0 min
@Temperature 23.3 °C
Shelf Life 10.0 MonthActivator (B side)
 10.0 MonthAdhesive (A side)
 10.0 MonthCartridges
 
Descriptive Properties
Fixture Time (mins)55 to 6074°F cure. Varies with bond gap and temperature.
Gap Filling (in)0.012 to 0.5Room temperature cure.
Mix Ratio by volume10 to 1Adhesive to Activator. Room temperature
Mix Ratio by weight8.86 to 1.0 or 1.02Adhesive to Activator. Room temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PITWP9006 / 239516

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.