MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

Akrochem Micral® 632 Flame retardant
Categories: Other Engineering Material

Material Notes: Product Description: Alumina Trihydrate (ATH or hydrated alumina) is a non-toxic, non-corrosive, flame retardant and smoke suppressant utilized in elastomeric applications. It is the most frequently used flame retardant in the world. ATH is a very effective flame retardant due to its thermodynamic properties which absorb heat and release water vapor. Alumina trihydrate releases its 35% water of crystallization as water vapor when heated above 205°C. The resulting endothermic reaction cools the product below flash point, reducing the risk of fire and acts as a vapor barrier to prevent oxygen from reaching the flame. Typical loadings vary from 20 phr to 150 phr. Because many polymers like polyethylene and polypropylene process above 200°C, these polyolefins should use magnesium hydroxide as a flame retardant filler since its water of hydration releases at approximately 325°C.

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Particle Size 3.5 µm3.5 µmMedian
Specific Surface Area 8.0 m²/g8.0 m²/g
 
Processing PropertiesMetricEnglishComments
Moisture Content 0.40 %
@Temperature 105 °C
0.40 %
@Temperature 221 °F
Free
 
Component Elements PropertiesMetricEnglishComments
Fe2O3 0.0070 %0.0070 %
Loss on Ignition(%) 34.6 %34.6 %
Na2O 0.30 %0.30 %
SiO2 0.0050 %0.0050 %
 
Descriptive Properties
Absorption32Oil
Content0.992Al(OH)3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PAKZCH237 / 315155

Visit Zeus Inc. for PEEK Tubing

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.