30% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C). ECO Conforming. US FDA Food Contact compliant in recognized colors. Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant,Food Contact Acceptable Information provided by SABIC |