MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Mitsubishi Chemical Advanced Materials TIVAR® CleanStat™ white UHMW-PE Ultra High Molecular Weight Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: TIVAR® CleanStat™ white UHMW-PE offers the electrostatic dissipative properties often required for UHMW-PE components operating at high line speeds and conveying rates. This TIVAR® CleanStat™ UHMW-PE White with permanent ESD properties and white color has specifically been developed for Food and Pharma Industry.

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.950 g/ccISO 1183-1
Water Absorption <= 0.10 %
@Time 86400 sec
immersion in water; ISO 62
Water Absorption at Saturation <= 0.10 %ISO 62
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 60ISO 868
Tensile Strength 18.0 MPaISO 527-1/-2
Elongation at Break >= 50 %ISO 527-1/-2
Elongation at Yield 11 %ISO 527-1/-2
Modulus of Elasticity 0.580 GPaISO 527-1/-2
Compressive Strength 5.80 MPa
@Strain 1 %
ISO 604
 9.70 MPa
@Strain 2 %
ISO 604
 15.9 MPa
@Strain 5.0 %
ISO 604
K Factor (ISO) 10 µm/kmISO 7148-2
Charpy Impact Unnotched NBISO 179-1/1eU
Charpy Impact, Notched 20.0 kJ/m²ISO 179-1/1eA
Coefficient of Friction, Dynamic 0.15 - 0.30QTM 55007
Limiting Pressure Velocity 0.0500 MPa-m/sec1 m/s cylindrical sleeve bearings
 0.0800 MPa-m/secat 0.1 m/s cylindrical sleeve bearings
 
Electrical PropertiesOriginal ValueComments
Surface Resistivity per Square 1.00e+8 - 1.00e+9 ohmANSI/ESD STM 11.11
Dielectric Constant 2.49
@Frequency 1e+6 Hz
ASTM D150
Dissipation Factor 0.028
@Frequency 1e+6 Hz
ASTM D150
 
Thermal PropertiesOriginal ValueComments
CTE, linear 220 µm/m-°C
@Temperature 23.0 - 100 °C
Thermal Conductivity 0.400 W/m-K
Melting Point 135 °C10°C / min; ISO 11357-1/-3
Maximum Service Temperature, Air 80.0 °C20,000 hours
Deflection Temperature at 1.8 MPa (264 psi) 40.0 °CISO 75-1/-2
Minimum Service Temperature, Air -200 °C
Flammability, UL94 HB
@Thickness 3.00 mm
Oxygen Index <= 20 %ISO 4589-1/-2
 
Descriptive Properties
ColorWhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

P1SM919 / 291076

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.