Compound 4762 is a 70 durometer blue colored Neoprene elastomer. This compound will meet or exceed the specifications listed and has the following physical properties: ASTM D2000 3 BC 715 A14 B14 EO14 EO34 G21; 5 BC 715 A14 B14 EO14 EO34 G21; 6 BC 715 A14 B14 EO14 EO34 G21; 2 BE 715 A14 EO14; 3 BE 715 A14 EO14 G21 Information provided by Pressure Seals Inc. |