MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
ASI® Threadlocker TORQUE 43 TL Anaerobic Dimethacrylate Ester Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: ADVANCED PERFORMANCE SERIES THREADLOCKER 43TL is a medium strength anaerobic adhesive for thread locking of nuts and bolts of all types that require to be dismantled. Suitable to be used on oily surfaces. Highly resistant to heat, corrosion, vibrations, water, gas, oils, hydrocarbons and many chemicals. Also to be used as a thread sealant in the temperature range -55° +150°C.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.08 g/cc
@Temperature 25.0 °C
uncured
Brookfield Viscosity 5000 cP
@Temperature 25.0 °C
Uncured. Spindle 3-20 rpm
Storage Temperature 8.00 - 28.0 °Cuncured
 
Thermal PropertiesOriginal ValueComments
CTE, linear 80.0 µm/m-°C@ 20° on steel 24 hrs; ASTM D696
Specific Heat Capacity 0.300 J/g-°C
@Time 86400 sec
20° on steel. Cured
Thermal Conductivity 0.100 W/m-K
@Time 86400 sec
20° on steel; ASTM C177
Maximum Service Temperature, Air 150 °C20°C on steel 24 hrs.
Minimum Service Temperature, Air -55.0 °C20°C on steel 24 hrs.
Flash Point >= 93.0 °Cuncured
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 20.0 °C
uncured
 
Descriptive Properties
Chemical ClassDimethacrylate Ester
Color / appearanceOpaque blue fluorescent liquid
Locking Torque14 to 34 N.m. Breakloose. 24 hrs @ 20° on steel. DIN 54454
 15 to 25 N.m. Breakaway. 24hrs @ 20° on steel. (ISO 10964) 4,3

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9174 / 233540

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.