MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
ChenGuang CGF-218K PTFE Powder
Categories: Polymer; Thermoplastic; Fluoropolymer; Polytetrafluoroethylene (PTFE)

Material Notes: Molecular Formula: [CF2--CF2]n

CAS No. 9002-84-0

Description: In addition to all excellent properties of PTFE material, CGF-218 series powders has outstanding performance in paste extrusion to manufacture sealing tape, etc.. The resin are processed by mixing them with some organic solvents to obtain paste which are made into coherent, smooth and flat semifinished products after ram extrusion. During this progression the extruding pressure remains steady .The semifinished products can be further processed to produce unsintered tape by calendering, elongating and removing solvent with heat, and also to manufacture sintered coherent thin-walled tubing , continuous long rod, and wire & cable coating, etc.

Main Applications: Oil-free unsintered broad tape for cutting apart

Extrudate appearance: flat, smooth and coherent

Information provided by ChenGuang Research Institute of Chemical Industry

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 2.19 - 2.25 g/cc
Bulk Density 0.320 - 0.520 g/cc
Particle Size 600 - 900 µm
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 23.0 MPa
Elongation at Break 300 %
 
Thermal PropertiesOriginal ValueComments
Melting Point 327 °C
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.040 %
 
Descriptive Properties
Heat Instability Index50

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHENGU033 / 255632

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.