MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Lord Adhesives 7550 Urethane Adhesive System
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Adhesive

Material Notes: LORD® 7550 adhesive is an equal-mix, two-component clear urethane adhesive system used to bond Lexan®, ABS, polycarbonate and other plastics. This adhesive will also bond primed metals. Lexan is a trademark of SABIC Innovative Plastics. After opening, protect adhesive from excessive exposure to moisture by installing desiccant cartridges and/or using dry nitrogen as an inert cover.

Features: does not require explosion-proof equipment. does not contain ozone depleting chemicals. resists sunlight, weathering, humidity and salt spray. solvent resistant when cured. Painting and most cleaning processes do not affect bond strength. flows into hard-to-reach spaces; excellent for bonding parts with tight tolerances.

All information provided by Lord.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 9.00 - 9.40 lb/galC Curative
 9.60 - 9.80 lb/galA Resin
Solids Content >= 100 %by weight, mixed with curative
Viscosity Measure 1800 - 4000 cSt
@Temperature 25.0 °C
A Resin
 6000 - 12500 cSt
@Temperature 25.0 °C
C Curative
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 93.0 °Cclosed cup
 
Processing PropertiesOriginal ValueComments
Pot Life 60.0 min
@Temperature 25.0 °C
time to handling strength, mixed with curative
Working Life 3.00 - 5.00 min
@Temperature 24.0 °C
Mixed with curative
Shelf Life 6.00 Month
@Temperature 21.0 - 27.0 °C
in original, unopened container
 
Descriptive Properties
AppearanceClear LiquidA Resin
 Clear LiquidC Curative
Mix Ratio1 to 1by volume, resin to curative
Processing Time2 to 3 min.Purge time, 24 C, mixed with curative

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLORD9135 / 232523

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.