MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Akrochem ZINC OXIDE 35
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Applications: Zinc Oxide 35 is an effective accelerator/activator of extremely fine particle size, suitable for rubber articles based on natural and synthetic elastomers, as well as for latex applications. The fine particle size and high activity of Zinc Oxide 35 permits a 40% reduction in the level of addition compared to regular zinc oxide grades. Moreover, it is useful in applications where only low concentrations of zinc oxide can be tolerated, e.g. transparent and translucent rubber goods. Employed at high levels, it provides good fatigue resistance and heat dissipation in dynamically stressed articles, such as buffers and rollers. Zinc Oxide 35 is also a crosslinking agent for metal oxide curable elastomers - for example polychloroprene (CR) and carboxylated lattices

Information provided by Akrochem Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 5.60 g/cc
Particle Mesh Size 230 Mesh<0.2% Residue
Specific Surface Area 45 m²/g
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd 0.00050 %
Copper, Cu 0.00050 %
Iron, Fe 0.0020 %
Lead, Pb 0.0010 %
Loss on Ignition(%) <= 4.0 %
Manganese, Mn 0.0010 %
 
Descriptive Properties
Appearancewhite to light yellow powder
Content>93%Zinc Oxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PAKZCH659 / 315577

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.