This high density polyethylene is an ethylene-hexene copolymer tailored for injection molded applications that require: • Good flow performance • Slip agent with good organoleptics and high oxidative stability • High impact strength • Excellent stiffness. Typical injection molded applications for 9012C include items such as: • Caps • Closures • Containers. information provided by Chevron Phillips Chemical Company LP. |