Lupolen GX 5038 is a new generation hexene linear high-density polyethylene for injection molding. Typical customer applications may include SCR reservoirs (SCR = Selective Catalytic Reduction). Lupolen GX 5038 is a pelletized polymer. It is not intended for use in medical and pharmaceutical applications. Applications: Non-fuel ReservoirsInformation provided by LyondellBasell. |