DANADD® TPU 91041-LASER is supplied as black laser additive batch. In general it must not be added further color masterbatches. When you want to achieve a dark black, we would recommend the addition of 1-2% of the TPU color masterbatch PEARLTHANE MB-9005. Application: DANADD® TPU 91041-LASER is added during the injection molding process together with TPU’ s in a mete-ring mixing unit. To the DANADD® combination laser additive batches it can be also added other additive batches for the UV protection or improvement of the hydrolysis resistance. Information provided by Danquinsa GMBH |