MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Ascend Performance Materials Vydyne® AG7K PA66-GF35
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 66 (PA66); Nylon 66, 40% Glass Fiber Filled

Material Notes: Vydyne AG7K is a glass fiber reinforced, heat and hydrolytically stabilized PA66 for injection molded applications.

Information provided by Ascend Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.42 g/ccDAM; ISO 1183
Water Absorption 0.80 %
@Temperature 23.0 °C,
Time 86400 sec
DAM; ISO 62
Moisture Absorption at Equilibrium 1.4 %DAM to 50% RH; ISO 62
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 155 MPa50% RH; ISO 527-2
 211 MPaDAM; ISO 527-2
Elongation at Break 3.5 %DAM; ISO 527-2
 4.3 %50% RH; ISO 527-2
Tensile Modulus 9200 MPa50% RH; ISO 527-2
 12500 MPaDAM; ISO 527-2
Flexural Strength 191 MPa50% RH; ISO 178
 308 MPaDAM; ISO 178
Flexural Modulus 8300 MPa50% RH; ISO 178
 11400 MPaDAM; ISO 178
Izod Impact, Notched (ISO) 11.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 180/1A
 12.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 180/1A
 13.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 180/1A
 14.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 180/1A
 14.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 180/1A
 17.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 180/1A
Charpy Impact Unnotched 87.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eU
 91.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eU
 102 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eU
 102 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eU
 107 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eU
 112 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eU
Charpy Impact, Notched 12.0 kJ/m²
@Temperature -40.0 °C
DAM; ISO 179/1eA
 12.0 kJ/m²
@Temperature -40.0 °C
50% RH; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
DAM; ISO 179/1eA
 13.0 kJ/m²
@Temperature -30.0 °C
50% RH; ISO 179/1eA
 16.0 kJ/m²
@Temperature 23.0 °C
DAM; ISO 179/1eA
 19.0 kJ/m²
@Temperature 23.0 °C
50% RH; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+16 ohm-cm
@Thickness 1.00 mm
DAM; IEC 60093
Dielectric Strength 29.0 kV/mm
@Thickness 1.00 mm
50% RH; IEC 60243
 30.0 kV/mm
@Thickness 1.00 mm
DAM; IEC 60243
 
Thermal PropertiesOriginal ValueComments
Melting Point 260 °CDAM; ISO 11357-3
Deflection Temperature at 0.46 MPa (66 psi) 261 °CUnannealed, 50% RH; ISO 75-2/B
 262 °CUnannealed, DAM; ISO 75-2/B
Deflection Temperature at 1.8 MPa (264 psi) 248 °CUnannealed, 50% RH; ISO 75-2/A
 253 °CUnannealed, DAM; ISO 75-2/A
UL RTI, Electrical 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical with Impact 65.0 °C
@Thickness 0.750 mm
UL 746
 65.0 °C
@Thickness 3.00 mm
UL 746
UL RTI, Mechanical without Impact 65.0 °C
@Thickness 3.00 mm
UL 746
Flammability, UL94 HB
@Thickness 0.750 mm
UL 94
 HB
@Thickness 3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Rear Barrel Temperature 260 - 280 °CInjection
Middle Barrel Temperature 270 - 280 °CInjection
Front Barrel Temperature 270 - 290 °CInjection
Melt Temperature 270 - 290 °CInjection
Mold Temperature 60.0 - 90.0 °CInjection
Drying Temperature 75.0 - 85.0 °C
Dry Time 4.00 hour
Moisture Content 0.20 %Injection
 
Descriptive Properties
AdditiveHeat Stabilizer
 Release agent
Agency RatingsISO, 1043 PA66 GF35
AppearanceBlack
 Natural Color
FeaturesGood Strength
 Outstanding Surface Finish
FormsPellets
Processing MethodInjection Molding

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASCE9255 / 287608

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.