2003 is a single component low viscosity cyanoacrylate adhesive, suitable for general-purpose applications on metals rubbers and plastics. 2003 is approved to ISO 10993-5 for biocompatibility, making it suitable for use in medical device applications.Information provided by H.B. Fuller Company |