MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
ASI® MP 52051 & MP 5212 Activator Methacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Methacrylate; Methacrylate Adhesive

Material Notes: MP 52051 is a two component no mix acrylic, curing by contact, does not require mixing. Fixture time is under 30 seconds on most substrates. This material has been engineered to bond a wide range of various metal substrates. The material forms a tough durable bond, able to withstand harsh environments, with excellent aging and weathering properties.

Information provided by Adhesive Systems, Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccUncured. MP 5212
 1.10 g/ccUncured. MP 52051
Viscosity 5.0 - 10 cP
@Temperature 25.0 °C
MP 5212
 15000 - 25000 cP
@Temperature 25.0 °C
MP 52051
Storage Temperature 0.000 - 30.0 °CMP 52051
 
Thermal PropertiesOriginal ValueComments
Flash Point >= 87.0 °CMP 5212
 >= 103 °CMP 52051
 
Processing PropertiesOriginal ValueComments
Shelf Life 12.0 Month
@Temperature 20.0 °C
MP 52051
 12.0 Month
@Temperature 20.0 °C
MP 5212
 
Descriptive Properties
Chemical ClassMethacrylate Ester. MP 5212
 Urethane Methacrylate. MP 52051
Color / appearanceAmber liquid. MP 5212
 Amber/Thixotropic. MP 52051

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PASINC9224 / 233590

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.