MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
En-Door ACR ED-401B PVC Processing Aid
Categories: Other Engineering Material

Material Notes: General Information: ED-401B is a medium-high molecular weight acrylic processing aid. It has good weather resistance, high impact-resisting strength, heat stability, and low percent thermal shrinkage, can promote plastication of PVC resin, decrease process temperature and bring excellent surface quality to finished products.

Application: ED-401B is a general purpose processing aid and suitable for PVC window and door profiles, pipes and fittings, etc. The recommended dosage is 1.0-2.0 phr for 100 phr PVC resin.

Information provided by En-Door

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.400 - 0.550 g/ccSurface
Volatiles <= 1.0 %
Particle Mesh Size 40 Mesh0.45mm, =98%, Granularity
Viscosity Measurement 4.8 - 5.3[?], Ubbelohde Viscometer
 
Descriptive Properties
AppearanceWhite powder

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PENDOOR034 / 316668

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.