MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Momentive Performance Materials GE Sealants & Adhesives MAX Shield Painter's Advanced Acrylic Latex Sealant
Categories: Polymer; Thermoset; Silicone

Material Notes: MAX Shield Painter Advanced Polymer Acrylic Latex is a premium sealant ideal for the most demanding paint projects inside and out. Formulated with Tri Shield Protection, this sealant is100% waterproof, and offers exceptional flexibility, excellent adhesion to a wide variety of building materials, and lifetime mold-free product protection. Max Shield sealant can span up to 2-inch gaps with over 600% stretch and 25% joint movement. This paint-friendly sealant is low in odor, guns out effortlessly, tools smoothly, and cleans-up easily with soap and water. The durable seal resists cracking, chalking, and crumbling in all seasons, and is guaranteed for sixty years.

Features: Tri-Shield Protection, 100% waterproof – can withstand severe weather and harsh environments, Excellent flexibility – can span up to 2-inch gaps with over 600% stretch and ± 25% Joint Movement, Mold free guarantee – cured caulk is resistant to mold and mildew growth, Paint Friendly – won’t cause paint to crack, fade or change sheen, Non-Staining – does not stain or discolor most substrate surfaces, Excellent adhesion to most common building materials, including most wood, metal, concrete, brick, plaster, masonry, glass and ceramic tile, Low odor and low VOC (Meets CARB VOC limits), Easy application, Soap and water clean-up.

Applications: Max* Shield Painter’s Advanced Polymer Acrylic Latex sealant can be used in a wide variety of interior and exterior applications including, but not limited to, trim, crown molding, baseboards, vents and around doors, windows.

Information provided by Momentive Performance Materials.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.41 g/ccUncured
Solids Content 74 - 78 %By weight. Uncured.; ASTM C1250
Volatile Organic Compounds (VOC) Content <= 47.5 g/lUncured. Excluding water & exempt compounds
 
Mechanical PropertiesOriginal ValueComments
Elongation at Break 620 %ASTM D412
Peel Strength 12.0 pliDry/wet.; ASTM C794
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 100 °F
Minimum Service Temperature, Air -40.0 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 100 °CApplication Temp
Cure Time 24.0 hour3/16 inch bead size
Tack-Free Time 60.0 minASTM C679
Shelf Life 24.0 Month
 
Descriptive Properties
AppearanceSmooth & CreamyUncured.
Artificial WeatheringPassedCured. ASTM C793
BaseAcrylic Latex
Carb Chem Curing VOC<1.5 wt.%Uncured. Non-Chem Curing.
Clean-upSoap & Water
ColorWhiteMAP410WT 12C, MAP405WT 12C
Consistency / SagPassedUncured. ASTM C693
Coverage Rate51 Lin. Ft.At 3/16" bead.
Cracking & CaulkingNone-passedASTM C792
Freeze/Thaw StabilityPassed / 5 Cycles at 0°FUncured. ASTM C731.
Joint Movement Capability±25%ASTM C719.
OdorSlight AcrylicUncured
Paint Ready Time30 minutes
PaintableLatex & Oil Based Paints
Stain/Color ChangePassedASTM C510
Water Ready24 hoursUncured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMOMEN9950 / 265762

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.