Low-viscosity, heat-and light-stabilized polyamide 12. VESTAMID® LX9034 is a low-viscosity, heat and light stabilized Nylon 12 for injection molding. The semi-crystalline compounds based on PA 12 have a low water absorption. Therefore manufactured parts exhibit excellent dimensional stability at changing ambient humidity, combined with constant high impact strength, a low coefficient of friction and good chemical resistance. VESTAMID® LX9034 is supplied as cylindrical granules, ready for processing, in moisture-proof bags. Pigmentation may affect values. Property data for dry samples. Information provided by Evonik. |